Red ceramic body in rectangular block format. Ideal for hand-building or use on the potter’s wheel. Highly malleable body, easy to shape. Soft hardness. The clay body should be properly sealed when not in use. This clay is not suitable for direct contact with flame. 12.5 kg packaging. Technical data sheet available for download.
– Dry mechanical strength: 95±10 kgf/cm²
– Mechanical strength after firing: 400±50 kgf/cm²
– Total shrinkage: 7.0±1.0 %
– Water absorption: 10.0±1.0 %
– Cubic thermal expansion coefficient (ΔT20–400 °C): (220 ± 5) × 10^-7 °C^-1
– Biscuit firing temperature: 980 °C (±10 °C)
– Glaze firing temperature: 1000 °C (±10 °C)